Air entraining plasticiser
Increases the durability to freeze and thaw action and also allows water reduction to the mix. The latter counteracts with the loss of strength that may result from air entrainment. It is ideal for prefabricated and normal concrete and for continuous extrusion of concrete such as the bumpers on highways.
COVERAGE | 0,10-0,16lt/50kg of cement |
TECHNICAL SHEET TSIRCO-FLOAIR No3